Content page
From [Institution name]
| Pressure (kPa) |
Requirement |
ResultFootnote (1) |
|---|---|---|
| 3 |
No evidence of deformation, permanent damage or failure |
Pass |
| 3.8 |
No evidence of deformation, permanent damage or failure |
Pass |
| 4.5 |
No evidence of deformation, permanent damage or failure |
Pass |
| 5.2 |
No evidence of deformation, permanent damage or failure |
Pass |
| 5.9 |
No evidence of deformation, permanent damage or failure |
Pass |
| 6.6 |
No evidence of deformation, permanent damage or failure |
Pass |
| 7.3 |
No evidence of deformation, permanent damage or failure |
Pass |
| 8.1 |
No evidence of deformation, permanent damage or failure |
Pass |
| 8.8 |
No evidence of deformation, permanent damage or failure |
Pass |
| 9.0Footnote (2) |
– |
Batten fastener pull-through |
| Wind Speed (km/h) |
Simulated Rainfall (L/m2•min) |
Duration (min) |
Requirement |
ResultFootnote (1) |
|---|---|---|---|---|
50 |
3.7 |
15 |
No leakage or damage |
Pass |
110 |
3.7 |
15 |
No leakage or damage |
Pass |
140 |
3.7 |
15 |
No leakage or damage |
Pass |
170 |
3.7 |
5 |
No leakage or damage |
Pass |
| Property |
Test Method |
Result |
|---|---|---|
| Stone coated steel |
ASTM B 117 |
Pass |
| Property |
Test Method |
Result |
|---|---|---|
| Granule adhesion |
ASTM D 4977 |
Pass |