Content page
From [Institution name]
Test |
Requirement |
Result |
---|---|---|
Five 1 m2 specimens were tested and measured for air permeance, before-and-after accelerated aging, at a minimum of six air pressure differentials (ΔP) between 0 and 250 Pa. |
Air leakage rate at 75 Pa ΔP (based on linear regression of 30 data points) ≤ 0.02 L/(s·m2) |
0.002 L/(s·m2) |
Property |
Unit |
Requirement |
Si-COAT® 422AB™ Result |
---|---|---|---|
WVP (applied over 12.7 mm DensGlass® at 25 ± 5 mils DFT thickness) |
ng/(Pa·s·m2) |
> 60 |
187 |