Content page
From [Institution name]
Property | Unit | Requirements |
---|---|---|
Measured thickness sheet–overall | mm | 1.016 |
Measured thickness coating over scrim or fabric | mm | 0.38 |
Breaking strength | N | ≥ 400 |
Dynamic puncture resistance | -- | Pass @ 10 J |
Static puncture resistance | -- | Pass @ 25 kg |
Elongation ultimate | % | ≥ 250 |
Elongation at fabric break ultimate - MD Footnote (1) | % | ≥ 15 |
Elongation at fabric break ultimate - XD Footnote (1) | % | ≥ 15 |
Tearing strength | ≥ 45 | |
Brittleness point | °C | –45 |
Ozone resistance, on cracks | -- | Pass |
Heat aging - breaking strength | N | ≥ 356 |
Heat aging - elongation, ultimate | % | ≥ 200 |
Heat aging - linear dimensional change | % | ≤ ± 1 |
Water absorption | mass % | ≤ +8, –2 of original |
Factory seam strength | kN/m | ≤ 8.8 |
Weather resistance - visual inspection | -- | No cracks or crazing |